TECHNINIŲ DUOMENŲ LAPAS
18.03.2010

Fontecoat EP 50 - Water-borne epoxy topcoat

 
Fontecoat_EP_50
APIBŪDINIMAS A two component waterborne epoxy topcoat and a single coat paint.
SAVYBĖS

Used as a topcoat or as a single coat paint in epoxy paint systems for steel surfaces. Can also be used as a primer or intermediate coat in epoxy / polyurethane systems. 

Paskirtis Recommended for framework, service platforms, conveyors and other steelwork, machinery and equipment.

TECHNINIAI DUOMENYS
Papildomos savybės Very good resistance against mechanical and chemical stress.
Spalvų katalogai TEMASPEED FONTE tinting.
Blizgumas Pusiau blizgus
Teorinė išeiga

Recommended film thicknesses

Theoretical coverage

dry

wet

 

60 µm

130 µm

7.7 m2/l

100 µm

210 µm

4.8 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Skiediklis Vanduo
Maišymo santykis Base 1 part by volume 168-series
Hardener 1 part by volume 007 1019
Įrankiai By airless spray or brush.
Mišinio tinkamumo trukmė (esant +23 ºC temperatūrai) 1½ h.
Džiūvimo laikas

DFT 100 µm

+ 15 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

4 h

2 h

1 h

Touch dry, after

8 h

5 h

2 h

Recoatable by itself, min. after

16 h

6 h

4 h

Recoatable without roughing, max. after

7 d

5 d

2 d

Fully cured, after

14 d

7 d

3 d


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Sausasis likutis 47 ± 2 volume % (ISO 3233)
62 ± 2 weight %
Tankis 1,4 kg/l (mixed).
Gaminio kodas 168 -series

NAUDOJIMO INSTRUKCIJA
Dengimo sąlygos All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +15ºC during application and drying. Relative humidity should not exceed 70%. The surface temperature of the steel should remain at least 3ºC above the dew point.
Paviršiaus paruošimas Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Priming Fontecryl APS, Fontezinc 85, Fontecoat EP Primer, Fontecoat EP 50, Temazinc 99 and Temacoat GPL-S Primer.
Viršutinio sluoksnio danga Fontecoat EP 50 and Fontedur HB 80.
Dažymas By airless spray or brush. If necessary, the paint can be thinned 0 - 10%. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 140 - 180 bar. Spray angle shall be chosen according to the shape of the object. 160 μm DFT should not be exceeded.
Komponentų maišymas First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Įrankių valymas Water or a mixture of water and Thinner 1029, 1:1. The equipment must be cleaned immediately after use before the paint dries.
Lakiųjų organinių junginių kiekis (LOJ) (direktyva 2004/42/EB) The Volatile Organic Compounds amount is 60 g/litre of paint mixture.
VOC content of paint mixture (thinned by 10 % by volume) 55 g/l.

Only for industrial and professional use.

SAUGOS IR SVEIKATOS APSAUGOS ŽENKLINIMAS
pagal reglamentą EB Nr. 1272/2008
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj.
Saugos duomenų lapasFontecoat EP 50
Kietiklio saugos duomenų lapasFontecoat EP 50
 
-


Atgal